This video shows how to use body lead instead of bondo. I only had 10 minutes so I put as much as I could that is important. Start with a clean, sanded surface so the tinning butter will bond correctly. This hood was from the 1969 Mustang restoration project from a few years ago. 90% of the body work on that car was done with lead. One you learn how you’ll never use bondo again!
Post time: Dec-06-2017